Related Books
Language: en
Pages: 202
Pages: 202
Type: BOOK - Published: 2017-01-20 - Publisher: BoD – Books on Demand
In this work Atomic Layer deposition of niobium and titanium doped ZnO based Transparent Conductive Oxide (TCO) coatings were developed. The fundamentals requir
Language: en
Pages: 453
Pages: 453
Type: BOOK - Published: 2007-12-29 - Publisher: Springer Science & Business Media
Zinc oxide (ZnO) belongs to the class of transparent conducting oxides that can be used as transparent electrodes in electronic devices or heated windows. In th
Language: en
Pages: 166
Pages: 166
Type: BOOK - Published: 2019-01-10 - Publisher: BoD – Books on Demand
Chemical vapor deposition (CVD) techniques have played a major role in the development of modern technology, and the rise of nanotechnology has further increase
Language: en
Pages: 317
Pages: 317
Type: BOOK - Published: 2020-05-07 - Publisher: CRC Press
Oxide-based materials and structures are becoming increasingly important in a wide range of practical fields including microelectronics, photonics, spintronics,
Language: en
Pages: 630
Pages: 630
Type: BOOK - Published: 2022-02-19 - Publisher: Elsevier
Nanomaterials via Single-Source Precursors: Synthesis, Processing and Applications presents recent results and overviews of synthesis, processing, characterizat