Related Books

Some Observations on the Electron-microscopic Fractography of Embrittled Sheets
Language: en
Pages: 28
Authors: W. R. Warke
Categories: Fractography
Type: BOOK - Published: 1964 - Publisher:

DOWNLOAD EBOOK

Observations on Delayed Cracking in Welded Structures of Unalloyed Titanium Sheet
Language: en
Pages: 12
Authors: R. H. Ernst
Categories: Titanium
Type: BOOK - Published: 1964 - Publisher:

DOWNLOAD EBOOK

A brief study of delayed fracture in a seam-welded titanium panel is summarized in this memorandum. Examination of the fracture surface with electron microscopy
The Production of Powder-metallurgy Tungsten Sheet and Plate
Language: en
Pages: 18
Authors: D. J. Maykuth
Categories: Powder metallurgy
Type: BOOK - Published: 1964 - Publisher:

DOWNLOAD EBOOK

Index to DMIC Reports and Memoranda
Language: en
Pages: 38
Authors: Battelle Memorial Institute. Defense Metals Information Center
Categories: Alloys
Type: BOOK - Published: 1968 - Publisher:

DOWNLOAD EBOOK

Continued Observations on the Distribution of Stress in the Vicinity of a Crack in the Center of a Plate
Language: en
Pages: 50
Authors: L. R. Jackson
Categories: Plates (Engineering)
Type: BOOK - Published: 1964 - Publisher:

DOWNLOAD EBOOK

This memorandum supplements and augments information presented in DMIC Memorandum 178 (AD-422 463). In the present report, Neuber's stress equations are rewritt