Structural Integrity of Fasteners Including the Effects of Environment and Stress Corrosion Cracking

Structural Integrity of Fasteners Including the Effects of Environment and Stress Corrosion Cracking
Author :
Publisher : ASTM International
Total Pages : 171
Release :
ISBN-10 : 9780803134133
ISBN-13 : 0803134134
Rating : 4/5 (33 Downloads)

Book Synopsis Structural Integrity of Fasteners Including the Effects of Environment and Stress Corrosion Cracking by : Pir M. Toor

Download or read book Structural Integrity of Fasteners Including the Effects of Environment and Stress Corrosion Cracking written by Pir M. Toor and published by ASTM International. This book was released on 2007 with total page 171 pages. Available in PDF, EPUB and Kindle. Book excerpt: Annotation Eleven peer-reviewed papers provide the latest information on the structural integrity of fasteners, including the effect s of environmental and stress corrosion cracking. For Sections cover:Fatigue and Crack Growth Experimental Techniques?three papers cover the development of a fastener structural element test for certifying navy fasteners material; experimental crack growth behavior for aerospace application; and influence of cold rolling threads before and after heat treatment on the fatigue resistance of high strength coarse thread bolts for multiple preload conditions. Design/Environmental Effects?two papers examined the relationship between the tightening speed with friction and clamped-load; and the optimum thread rolling process that improves SCC resistance to improve quality of design. Fatigue and Crack Growth Analytical Techniques?three papers describe current analytical techniques for fatigue and crack growth evaluations of fasteners; a numerical crack growth model using the finite element analysis generated stress field; and s the resistance of high strength fine thread bolts for multiple preload conditions. Design Consideration?focuses on the comprehensive nonlinear 3D finite element model to simulate a displacement controlled for riveted structure; state-of-the-art fatigue crack growth analysis techniques which are used in various industries to damage tolerance evaluation of structures; and the material stress state within the thread of the bolt; and on each parameter affecting the structural integrity of a bolted joint.


Structural Integrity of Fasteners Including the Effects of Environment and Stress Corrosion Cracking Related Books

Structural Integrity of Fasteners Including the Effects of Environment and Stress Corrosion Cracking
Language: en
Pages: 171
Authors: Pir M. Toor
Categories: Fasteners
Type: BOOK - Published: 2007 - Publisher: ASTM International

DOWNLOAD EBOOK

Annotation Eleven peer-reviewed papers provide the latest information on the structural integrity of fasteners, including the effect s of environmental and stre
Plating and Surface Finishing
Language: en
Pages: 416
Authors:
Categories: Electroplating
Type: BOOK - Published: 2007 - Publisher:

DOWNLOAD EBOOK

Scientific and Technical Aerospace Reports
Language: en
Pages: 892
Authors:
Categories: Aeronautics
Type: BOOK - Published: 1994 - Publisher:

DOWNLOAD EBOOK

ASTM Standardization News
Language: en
Pages: 844
Authors: American Society for Testing and Materials
Categories: Standardization
Type: BOOK - Published: 2004 - Publisher:

DOWNLOAD EBOOK

Structural Integrity of Fasteners
Language: en
Pages: 208
Authors: Pir M. Toor
Categories: Fasteners
Type: BOOK - Published: 1995 - Publisher: ASTM International

DOWNLOAD EBOOK