Role of Hydrogen in Hot-salt Stress-corrosion of a Titanium Alloy
Author | : Hugh R. Gray |
Publisher | : |
Total Pages | : 36 |
Release | : 1971 |
ISBN-10 | : UIUC:30112106691923 |
ISBN-13 | : |
Rating | : 4/5 (23 Downloads) |
Book Synopsis Role of Hydrogen in Hot-salt Stress-corrosion of a Titanium Alloy by : Hugh R. Gray
Download or read book Role of Hydrogen in Hot-salt Stress-corrosion of a Titanium Alloy written by Hugh R. Gray and published by . This book was released on 1971 with total page 36 pages. Available in PDF, EPUB and Kindle. Book excerpt: Hydrogen embrittlement during hot salt, stress corrosion of titanium alloys.